{"title":"Ceramic shell \u0026 investment","description":"\u003ch2 style=\"color: #1d71b8;\"\u003eCeramic shell and plaster investment for lost wax casting\u003c\/h2\u003e\n\u003cp\u003eTo cast bronze, aluminium or glass using the lost wax process, you build a refractory mould around the wax model. There are two ways to do this.\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003ca href=\"\/en\/collections\/keramische-schaal-materialen-voor-de-verloren-was-methode\"\u003eCeramic shell\u003c\/a\u003e:\u003c\/strong\u003e you build up a thin, light shell layer by layer with slurry and stucco. Quick to burn out and light in weight, but the slurry needs daily maintenance. Ideal if you cast regularly.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003ca href=\"\/en\/collections\/inbedmassa-gips-verloren-was\"\u003ePlaster investment\u003c\/a\u003e:\u003c\/strong\u003e you mix a batch each time and pour or apply a solid plaster mould around the model. Simple and with no slurry to maintain, but the mould is heavier and needs a longer burnout. HYDRACAST for metal, Crystalcast M248 for glass.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003eNot sure which route suits your casting project? Email us at \u003ca href=\"mailto:info@siliconesandmore.com\"\u003einfo@siliconesandmore.com\u003c\/a\u003e and we will be happy to advise you.\u003c\/p\u003e","products":[{"product_id":"diy-starterkit-easy-slurry-en-bezanding","title":"Starter Kit DIY Easy Slurry and Stucco","description":"\u003ch3\u003eDIY Easy Slurry\u003c\/h3\u003e\n\u003cp\u003eThis set contains all ingredients to make approximately 30 litres of periodically mixed, Shellspen-based slurry for the ceramic shell method yourself, including stucco.\u003c\/p\u003e\n\u003cp\u003eThe slurry does not need to stand in a continuously rotating tank, but it does require a fixed mixing schedule: mix for about half an hour on every day of use, and at least twice a week during periods without use. Never leave the slurry unmixed for more than 7 days.\u003c\/p\u003e\n\u003cp\u003eThe set gives you full control over the recipe. The individual ingredients keep for a long time when unmixed (see the date on the packaging).\u003c\/p\u003e\n\u003cp\u003eThe starter kit contains:\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\u003ca href=\"\/en\/products\/adbond-advantage\"\u003e1 x 25 kg jerrycan Adbond Advantage\u003c\/a\u003e\u003c\/li\u003e\n\u003cli\u003e1 x 25 kg fused silica flour 325 mesh\u003c\/li\u003e\n\u003cli\u003e1 x bag of Shellspen powder (suspension agent)\u003c\/li\u003e\n\u003cli\u003e1 x bottle of drying indicator (optional; dose a maximum of 100 ml per 25 kg Adbond)\u003c\/li\u003e\n\u003cli\u003e1 x 25 kg aluminium silicate sand, fine grain (0.2–0.5 mm)\u003c\/li\u003e\n\u003cli\u003e1 x 25 kg aluminium silicate sand, coarser grain (0.5–1.0 mm)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eAdvantages\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003eNo rotating slurry tank required: dip the model directly into a sealable container.\u003c\/li\u003e\n\u003cli\u003ePeriodic mixing according to schedule instead of continuous mixing.\u003c\/li\u003e\n\u003cli\u003eMinimal waste: close the container after use and store it within the temperature limits.\u003c\/li\u003e\n\u003cli\u003eEasy to adapt to your own requirements.\u003c\/li\u003e\n\u003cli\u003eCan be used as both primary and back-up slurry.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eImportant\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\u003cstrong\u003eStorage:\u003c\/strong\u003e Adbond binder at 5–30 °C, the prepared slurry at 15–25 °C (never below 5 °C or above 30 °C). Store frost-free; frozen binder or slurry is irreparably damaged.\u003c\/li\u003e\n\u003cli\u003e\u003cstrong\u003eMixing time when preparing:\u003c\/strong\u003e at least 4 hours, preferably 24 hours, with a mixer of no more than 2000 revolutions per minute.\u003c\/li\u003e\n\u003cli\u003e\u003cstrong\u003epH always above 9.5\u003c\/strong\u003e, measured with a pH meter.\u003c\/li\u003e\n\u003cli\u003e\u003cstrong\u003eAdjusting:\u003c\/strong\u003e thicken with flour plus the corresponding Shellspen, thin with Adbond. Use demineralised water only, and only to top up evaporated water.\u003c\/li\u003e\n\u003cli\u003e\u003cstrong\u003eDrying indicator:\u003c\/strong\u003e is a salt that makes the slurry less stable. Only use it when really necessary, and never more than 100 ml per 25 kg Adbond. Not recommended for beginners.\u003c\/li\u003e\n\u003cli\u003eThis set is intended for professional users. Read the manual in full before you start and pass it on to your customer if you resell the set.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eAluminium silicate\u003c\/h3\u003e\n\u003cp\u003eAluminium silicate is a good choice for the art caster. This product is mined in Europe, making it cheaper and more environmentally friendly. The shells are strong and reproduce the details of your artwork accurately. A shell with aluminium silicate has excellent refractoriness and high temperature stability.\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003eIncreased hot strength\u003c\/li\u003e\n\u003cli\u003eRobust and resilient\u003c\/li\u003e\n\u003cli\u003eEasy knock-out\u003c\/li\u003e\n\u003cli\u003eIncreased strength compared to fused silica systems\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eManual\u003c\/h3\u003e\n\u003cp\u003e\u003ca href=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/Manual_periodically_mixed_slurry_shellspen_EN_d8ed81e9-56b4-44d9-a0ea-a03ea3f9a7b9.pdf?v=1792407027\" target=\"_blank\" rel=\"noopener\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/pdf-download-small-v2.png?v=1726531275\" alt=\"\" width=\"50\" height=\"50\"\u003e\u003c\/a\u003e \u003ca href=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/Manual_periodically_mixed_slurry_shellspen_EN_d8ed81e9-56b4-44d9-a0ea-a03ea3f9a7b9.pdf?v=1792407027\" target=\"_blank\" rel=\"noopener\"\u003eManual for periodically mixed slurry based on Shellspen (PDF)\u003c\/a\u003e\u003c\/p\u003e","brand":"Nedform","offers":[{"title":"Request a quote","offer_id":49531856781653,"sku":"","price":0.0,"currency_code":"EUR","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/nedform-starterkit-diy-easy-slurry-en-bezanding-48098032451925.png?v=1727352436"},{"product_id":"burst-rsd-100","title":"Remet Burst 100 Antifoam – Fast Defoamer for Ceramic Shell Slurries \u0026 Binders","description":"\u003ch2\u003eFast defoamer for ceramic shell slurries\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eBurst 100 Antifoam\u003c\/strong\u003e is a non-ionic silicone defoamer for ceramic shell slurries. It breaks down foam quickly and lets trapped air bubbles escape fast. Burst 100 is compatible with many wetting agents and works in both alkaline and acidic binder systems. Before use, you dilute it 1 to 9 with deionised or distilled water. For longer-term foam control, you can combine Burst 100 with Remet's Foamaway.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eFast foam breakdown:\u003c\/strong\u003e air bubbles escape from the slurry quickly.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eAcidic and alkaline:\u003c\/strong\u003e works in both types of binder system.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eBroadly compatible:\u003c\/strong\u003e with most non-ionic, anionic and cationic agents.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eSuitable for latex binders:\u003c\/strong\u003e and for slurries with powerful wetting agents.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eLow dosage:\u003c\/strong\u003e a small amount of diluted emulsion is enough.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ New and existing ceramic shell slurries\u003c\/li\u003e\u003cli\u003e✓ Slurries with latex binder and powerful wetting agents\u003c\/li\u003e\u003cli\u003e✓ Investment casting and art casting\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eApplication\u003c\/h3\u003e\u003col\u003e\u003cli\u003eDilute: by hand or with a very slow-running mixer, add 1 part Burst 100 to 9 parts cold (16 to 32 °C) deionised or distilled water. Do not overmix, or the emulsion may partly break down.\u003c\/li\u003e\u003cli\u003eNew slurry: add up to 0.20 vol.% diluted antifoam to the liquid portion before adding the flour. That is about 2 ml per litre.\u003c\/li\u003e\u003cli\u003eExisting slurry: start with 5 to 20 ml diluted Burst 100 for a total volume of up to about 190 litres, and 10 to 40 ml for larger volumes.\u003c\/li\u003e\u003cli\u003eAdd the diluted antifoam slowly while mixing well. Otherwise it may float as an oily patch on the slurry and reach the wax, which impairs wetting.\u003c\/li\u003e\u003cli\u003eTwo smaller additions a few hours apart are better than one large addition.\u003c\/li\u003e\u003cli\u003eDiscard any diluted emulsion you do not use within 24 to 36 hours.\u003c\/li\u003e\u003c\/ol\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ The amount needed depends on binder, flour, additives and mixing procedure. Your practical experience determines the right dosage.\u003c\/li\u003e\u003cli\u003e✓ Burst 100 is sensitive to temperatures below 5 °C and above 40 °C. Protect it from frost.\u003c\/li\u003e\u003cli\u003e✓ If the product has been frozen, let it thaw, stir it well and test it before use, for example for its effect on the surface tension of colloidal silica.\u003c\/li\u003e\u003cli\u003e✓ Stable for up to 1 year in a closed container at 20 °C.\u003c\/li\u003e\u003cli\u003e✓ This product is intended for the business market. For larger quantities or custom solutions, email info@siliconesandmore.com.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eStruggling with foam in your slurry or unsure about the dosage? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"Remet","offers":[{"title":" 1 kg.  B2B","offer_id":49531872674133,"sku":"S10927","price":19.95,"currency_code":"EUR","in_stock":false},{"title":"4 Kg B2B","offer_id":49531872739669,"sku":"A10228","price":60.0,"currency_code":"EUR","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/remet-burst-rsd-100-48098044674389.jpg?v=1727353138"},{"product_id":"victawet","title":"Victawet 12 Wetting Agent – Better Slurry-to-Wax Adhesion for Ceramic Shell","description":"\u003ch2\u003eWetting agent for better slurry adhesion to wax\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eVictawet 12\u003c\/strong\u003e is a non-ionic, low-foaming organic phosphate ester. You use it as a wetting agent in ceramic shell slurries, with both acidic and alkaline binders. Victawet 12 helps the slurry adhere better to the wax surface. It is a 100% active liquid with a specific gravity of 1.12.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eBetter wax adhesion:\u003c\/strong\u003e the slurry wets the wax pattern evenly.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eVersatile:\u003c\/strong\u003e works in acidic and alkaline binders.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eLow foam:\u003c\/strong\u003e non-ionic and low-foaming.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eLow dosage:\u003c\/strong\u003e normally below 0.75% by volume.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Primary slurries for ceramic shell\u003c\/li\u003e\u003cli\u003e✓ Investment casting and art casting\u003c\/li\u003e\u003cli\u003e✓ Slurries based on colloidal silica\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing\u003c\/h3\u003e\u003col\u003e\u003cli\u003eBefore use, measure the pH of a 0.5% solution of Victawet 12.\u003c\/li\u003e\u003cli\u003eAdd 0.25% by volume to primary slurries, based on the total binder liquid (binder plus concentrate plus any dilution water).\u003c\/li\u003e\u003cli\u003eCheck that the slurry wets the wax parts properly. If not, add more in 0.05% increments until wetting is satisfactory.\u003c\/li\u003e\u003cli\u003eNormally stay below 0.75% by volume.\u003c\/li\u003e\u003cli\u003eAlways use Victawet 12 together with an effective anti-foam, such as \u003ca href=\"\/en\/products\/burst-rsd-100\"\u003eBurst 100\u003c\/a\u003e.\u003c\/li\u003e\u003c\/ol\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Victawet 12 hydrolyses over time, producing an acid.\u003c\/li\u003e\u003cli\u003e✓ Do not add it to alkaline colloidal silica if the pH of the 0.5% solution has dropped below approx. 3.0 to 3.5. It is still safe to use with LUDOX SK grades.\u003c\/li\u003e\u003cli\u003e✓ Causes serious eye irritation. Wear eye protection and protective clothing.\u003c\/li\u003e\u003cli\u003e✓ This product is intended for the business market. For larger quantities or custom requirements, email info@siliconesandmore.com.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure about the dosage in your own slurry or binder? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"Remet","offers":[{"title":"250 Gram B2B","offer_id":49531875754325,"sku":"S10926","price":57.0,"currency_code":"EUR","in_stock":true},{"title":"1 Kg B2B","offer_id":49531875819861,"sku":"A10449","price":114.68,"currency_code":"EUR","in_stock":true},{"title":"4 Kg B2B","offer_id":52583912800597,"sku":null,"price":400.0,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/remet-victawet-12-48098044641621.jpg?v=1727353138"},{"product_id":"crystalcast","title":"GRS Crystalcast M248 – Plaster-Bonded Investment for Glass Casting \u0026 Pâte de Verre","description":"\u003ch2\u003ePlaster-bonded investment for glass casting\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eGRS Crystalcast M248\u003c\/strong\u003e is a plaster-bonded investment specifically designed for casting glass and crystal. Its refractory content and permeability allow firing cycles up to 900 °C, for as long as 10 days depending on mould size. The mould has high strength during firing, yet comes away from the casting very easily once cool, so even filigree work can be removed without breakage. Its fine particle size distribution reproduces every detail with an exceptional surface finish. Crystalcast is suitable for small to large glass sculptures.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eFor glass casting:\u003c\/strong\u003e developed specifically for glass, crystal and pâte de verre.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eHeat resistant:\u003c\/strong\u003e firing cycles up to 900 °C and up to 10 days.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eStrong during firing:\u003c\/strong\u003e the mould holds its shape.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eEasy to remove:\u003c\/strong\u003e once cool, the mould comes away without risk of breaking the glass.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eFine detail:\u003c\/strong\u003e an exceptional surface finish, even on filigree work.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eSmall to large:\u003c\/strong\u003e suitable for small to large sculptures.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eExperience from practice\u003c\/h3\u003e\u003cp\u003eA glass artist in Germany carried out two glass casting projects, one with Crystalcast M248 and one with another, fast-setting glass casting investment (mixing ratio 29 : 100). His findings with M248:\u003c\/p\u003e\u003cul\u003e\u003cli\u003e✓ \u003cstrong\u003eMore user-friendly:\u003c\/strong\u003e because it sets less quickly, you have more time to mix and pour.\u003c\/li\u003e\u003cli\u003e✓ \u003cstrong\u003eEasier to degas:\u003c\/strong\u003e thanks to the higher water content (32 : 100) the mix can be vacuumed faster and better, even in a studio.\u003c\/li\u003e\u003cli\u003e✓ \u003cstrong\u003eLess material needed\u003c\/strong\u003e for the same mould.\u003c\/li\u003e\u003cli\u003e✓ \u003cstrong\u003eFiner glass surface:\u003c\/strong\u003e the glass came out of the mould smoother.\u003c\/li\u003e\u003cli\u003e✓ \u003cstrong\u003eSofter when demoulding:\u003c\/strong\u003e the mould comes away easily and smoothly.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Glass and crystal casting using the lost wax method\u003c\/li\u003e\u003cli\u003e✓ Pâte de verre\u003c\/li\u003e\u003cli\u003e✓ Finely detailed glass objects and filigree work\u003c\/li\u003e\u003cli\u003e✓ Small to large glass sculptures\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing (per the GRS TDS)\u003c\/h3\u003e\u003col\u003e\u003cli\u003eWeigh water and powder accurately in a 32 : 100 ratio. Always add the powder to the water.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eVacuum mixing:\u003c\/strong\u003e mix under vacuum for 5 minutes, pour the flasks in 2 minutes and hold under vacuum for 1 minute. About 8 minutes in total.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eConventional mixing:\u003c\/strong\u003e mix for 4 minutes, vacuum the bowl for 1 minute, then pour and vacuum the flasks in 3 minutes. About 8 minutes in total.\u003c\/li\u003e\u003cli\u003eLet the mould cure for at least 3 hours.\u003c\/li\u003e\u003cli\u003eRemove the wax with steam. This can take up to about 4 hours depending on mould size. Do not steam too long, as this can damage the mould surface.\u003c\/li\u003e\u003cli\u003eFill the mould with glass crystals, directly on the mould or in a ceramic feeder on top, and place it in a cold oven.\u003c\/li\u003e\u003cli\u003eFiring cycle: ramp up at no more than 50 °C per hour to 850 °C and hold for about 30 hours depending on mould size. The molten glass flows into the voids under gravity.\u003c\/li\u003e\u003cli\u003eCool the mould in the furnace at no more than 10 °C per hour to ambient temperature. Then gently remove the mould. Never quench glass or crystal castings.\u003c\/li\u003e\u003c\/ol\u003e\u003cp\u003eSee the \u003ca href=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/GRS_Crystalcast_Datasheet.pdf?v=1795699772\" target=\"_blank\"\u003eGRS Crystalcast technical data sheet (PDF)\u003c\/a\u003e for the burnout graph.\u003c\/p\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Crystalcast is intended for glass. For bronze and other metals, use \u003ca href=\"\/en\/products\/hydracast-tradition\"\u003eHYDRACAST Tradition\u003c\/a\u003e or \u003ca href=\"\/en\/products\/creart\"\u003eHYDRACAST Cre'Art\u003c\/a\u003e, see all \u003ca href=\"\/en\/collections\/plaster-investment-lost-wax-casting\"\u003einvestments for lost wax casting\u003c\/a\u003e.\u003c\/li\u003e\u003cli\u003e✓ The powder can release dust containing crystalline silica. Work with as little dust as possible, with extraction or good ventilation, and wear a dust mask (FFP2 or FFP3).\u003c\/li\u003e\u003cli\u003e✓ Store the powder dry and frost-free.\u003c\/li\u003e\u003cli\u003e✓ Supplied in 22.5 kg bags.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure which investment or firing cycle suits your model? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"GRS Goodwin","offers":[{"title":"Crystalcast 22.5 kg","offer_id":49531875852629,"sku":"A10708","price":79.95,"currency_code":"EUR","in_stock":false},{"title":"Quotation for outside BeNeLux and Germany","offer_id":49531875885397,"sku":"","price":0.0,"currency_code":"EUR","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/grs-goodwin-crystalcast-m248-48098049065301.jpg?v=1727353366"},{"product_id":"remasil-50","title":"Remet Remasil 50 Aluminosilicate – Stucco \u0026 Flour for Strong Ceramic Shells","description":"\u003ch2\u003eAluminosilicate stucco and flour for strong ceramic shells\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eRemet Remasil 50\u003c\/strong\u003e is a refractory aluminosilicate for building ceramic shells in investment and art casting. You can choose stucco in two grain sizes, 16\/30 mesh and 30\/60 mesh, and flour at 200 mesh. The stucco is custom ground into a uniform product with a narrow particle size range and few fines. This improves the permeability of the shell.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eStronger than fused silica:\u003c\/strong\u003e more strength than shells based on fused silica.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eHigh hot strength:\u003c\/strong\u003e robust and resilient during casting.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eEasy knockout:\u003c\/strong\u003e the shell is easy to remove after casting.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eLow dust:\u003c\/strong\u003e narrow particle size range with minimal fines, for better permeability.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eTwo grain sizes:\u003c\/strong\u003e so you can build the shell efficiently.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Stuccoing ceramic shells\u003c\/li\u003e\u003cli\u003e✓ Flour for making slurry\u003c\/li\u003e\u003cli\u003e✓ Investment casting and art casting\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing\u003c\/h3\u003e\u003col\u003e\u003cli\u003eDip the wax pattern in the slurry, for example a slurry based on \u003ca href=\"\/en\/products\/adbond-advantage\"\u003eRemasol Adbond Advantage\u003c\/a\u003e, and let the excess drain off.\u003c\/li\u003e\u003cli\u003eStucco the wet coat with the finer 30\/60 mesh stucco.\u003c\/li\u003e\u003cli\u003eLet each coat dry well before applying the next.\u003c\/li\u003e\u003cli\u003eBuild up the shell to the desired thickness with the coarser 16\/30 mesh stucco.\u003c\/li\u003e\u003cli\u003eUse the 200 mesh flour as a refractory filler when making your own slurry.\u003c\/li\u003e\u003c\/ol\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ This product is intended for the business market. For larger quantities or custom requirements, email info@siliconesandmore.com.\u003c\/li\u003e\u003cli\u003e✓ Avoid breathing in dust when pouring and stuccoing. Use extraction or wear respiratory protection.\u003c\/li\u003e\u003cli\u003e✓ Store the bags dry and closed.\u003c\/li\u003e\u003cli\u003e✓ Supplied in 25 kg bags.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eWould you like advice on building your shell or choosing between the grain sizes? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"Remet","offers":[{"title":"16-30 mesh. 25 kg. B2B","offer_id":49531876737365,"sku":"A10201","price":85.0,"currency_code":"EUR","in_stock":true},{"title":"30-60 mesh. 25 kg. B2B","offer_id":49531876802901,"sku":"A10202","price":85.0,"currency_code":"EUR","in_stock":true},{"title":"Flour 200 mesh. 25 kg.  B2B","offer_id":49531876868437,"sku":"A10203","price":85.0,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/remet-remasil-50-aluminosilicaat-stukko-en-meel-48098049786197.png?v=1727353414"},{"product_id":"fused-silica-lht-nl","title":"Remet Fused Silica LHT – Low-Expansion Refractory Flour \u0026 Sand for the Ceramic Shell","description":"\u003ch2\u003eLow-expansion refractory flour and sand for the ceramic shell\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eRemet Fused Silica LHT\u003c\/strong\u003e is very pure fused silica for building the ceramic shell. The material has low thermal expansion, excellent thermal shock resistance and low thermal conductivity. It is light and highly permeable, and the shell is easy to remove after casting. It is used for bronze, aluminium and steel. It is available as flour in 325, 200 and 120 mesh and as sand in 50\/100, 20\/50 and 10\/20 mesh.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eLow thermal expansion:\u003c\/strong\u003e a dimensionally stable shell at high temperature.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eExcellent thermal shock resistance:\u003c\/strong\u003e the shell copes well with rapid temperature changes.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eGood insulator:\u003c\/strong\u003e low thermal conductivity.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eLight and permeable:\u003c\/strong\u003e a lightweight shell with high gas permeability.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eEasy knock-out:\u003c\/strong\u003e the shell is easy to remove after casting.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eVery pure:\u003c\/strong\u003e for a long slurry life.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Flour for ceramic shell slurries\u003c\/li\u003e\u003cli\u003e✓ Sand for stuccoing the shell coats\u003c\/li\u003e\u003cli\u003e✓ Investment and art casting of bronze, aluminium and steel\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing\u003c\/h3\u003e\u003col\u003e\u003cli\u003eMix the flour with a binder, for example \u003ca href=\"\/en\/products\/adbond-advantage\"\u003eRemasol Adbond Advantage\u003c\/a\u003e, to make a slurry.\u003c\/li\u003e\u003cli\u003eDip the wax pattern into the slurry, let it drain and stucco the wet coat with fused silica sand.\u003c\/li\u003e\u003cli\u003eUse a coarser grain for each subsequent coat. This increases shell strength while keeping good gas permeability.\u003c\/li\u003e\u003cli\u003eLet each coat dry thoroughly before applying the next.\u003c\/li\u003e\u003c\/ol\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Avoid creating dust when pouring and mixing flour and sand, and do not breathe in the dust.\u003c\/li\u003e\u003cli\u003e✓ Store the material dry and in its closed packaging.\u003c\/li\u003e\u003cli\u003e✓ Other mesh sizes and larger quantities are available on request.\u003c\/li\u003e\u003cli\u003e✓ This product is intended for the business market. For larger quantities or custom solutions, email info@siliconesandmore.com.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure which grain size to use for each coat? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"Remet","offers":[{"title":"RG3 Sand  10\/20 Mesh 25 Kg. B2B","offer_id":49531879424341,"sku":"A10117","price":107.65,"currency_code":"EUR","in_stock":true},{"title":"RG2 Sand 20\/50 Mesh 25 Kg. B2B","offer_id":49531879457109,"sku":"A10116","price":83.95,"currency_code":"EUR","in_stock":true},{"title":"RG1 Sand  50\/100 Mesh 25 kg. B2B","offer_id":49531879489877,"sku":"A10115","price":83.95,"currency_code":"EUR","in_stock":true},{"title":"RP2 Flour 120 mesh 25 kg. B2B","offer_id":49531879391573,"sku":"A10114","price":107.65,"currency_code":"EUR","in_stock":true},{"title":"RP1 Flour 200 mesh 25 kg. B2B","offer_id":49531879358805,"sku":"A10113","price":107.65,"currency_code":"EUR","in_stock":true},{"title":"Fused silica flour 325 Mesh [25 kg]","offer_id":49923684532565,"sku":"A11963","price":84.0,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/remet-fused-silica-lht-meel-en-zand-48098049229141.jpg?v=1727353390"},{"product_id":"adbond-advantage","title":"Remet Remasol Adbond Advantage – Ready-to-Use Primary Binder for Ceramic Shell \u0026 Investment Casting","description":"\u003ch2\u003eReady-to-use primary binder for the ceramic shell\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eRemet REMASOL® ADBOND® Advantage\u003c\/strong\u003e is a ready-to-use, water-based binder for making the slurry for the ceramic shell. Thanks to its increased adhesion to wax surfaces, it is an ideal primary binder. The silica and polymer levels have been optimised for maximum adhesion, strength and elasticity, and a wetting agent and antifoam have already been added.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eExcellent adhesion to wax:\u003c\/strong\u003e the primary coat bonds well to the wax pattern.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eFewer defects:\u003c\/strong\u003e helps prevent common primary coat defects such as cracking and buckling.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eReady to use:\u003c\/strong\u003e wetting agent and antifoam are already added.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eBroadly compatible:\u003c\/strong\u003e with the refractories commonly used in primary slurries, such as fused silica, zircon and alumina.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eStable:\u003c\/strong\u003e stable pH and long slurry life.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eBetter permeability:\u003c\/strong\u003e improves the gas permeability of the shell.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eRobust:\u003c\/strong\u003e works well under less-than-ideal drying, environmental and processing conditions.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Primary slurry for the ceramic shell\u003c\/li\u003e\u003cli\u003e✓ Investment casting and art casting\u003c\/li\u003e\u003cli\u003e✓ Slurries with \u003ca href=\"\/en\/products\/fused-silica-lht-en\"\u003efused silica\u003c\/a\u003e, zircon or alumina\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing\u003c\/h3\u003e\u003col\u003e\u003cli\u003eUse the binder as supplied; you do not need to add wetting agent or antifoam.\u003c\/li\u003e\u003cli\u003eMix the binder with the refractory flour of your choice to make a primary slurry.\u003c\/li\u003e\u003cli\u003eApply the slurry as the first coat on the wax pattern and build up the shell according to your own process.\u003c\/li\u003e\u003cli\u003eFeel free to ask us about mix ratios and shell build-up.\u003c\/li\u003e\u003c\/ol\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Store the binder between 5 °C and 30 °C and protect it from frost.\u003c\/li\u003e\u003cli\u003e✓ To prevent frost damage, we only ship this product when the outside temperature is above 5 °C.\u003c\/li\u003e\u003cli\u003e✓ This product is intended for the business market. For larger quantities or custom solutions, email info@siliconesandmore.com.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure about the composition of your slurry or the build-up of your ceramic shell? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"Remet","offers":[{"title":" 5 kilo \/ 4.27 liter B2B","offer_id":49531880440149,"sku":"S10668","price":37.8,"currency_code":"EUR","in_stock":false},{"title":"25 kilos \/ 21.37 liters B2B","offer_id":49531880472917,"sku":"S10678","price":173.95,"currency_code":"EUR","in_stock":true},{"title":"240 kg. \/ 205.13 liters B2B","offer_id":49531880505685,"sku":"A10353","price":1393.92,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/remet-adbond-advantage-48098049294677.jpg?v=1727353390"},{"product_id":"hydracast-tradition","title":"GRS HYDRACAST Tradition – Refractory Investment for Lost Wax, Aluminium \u0026 Bronze","description":"\u003ch2\u003eRefractory investment for the traditional lost-wax method\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eGRS HYDRACAST Tradition\u003c\/strong\u003e is a ready-to-use refractory investment for art casters working with the traditional lost-wax method. You apply it by hand or machine directly onto the wax model. Use it as the first contact layer, or with added fillers such as grog or aluminosilicates as a reinforcing layer. This lets you build moulds from 15 cm to 2.5 metres for aluminium to bronze. You mix the powder with 42% water by weight and have a working time of approx. 13 minutes.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eTraditional lost wax:\u003c\/strong\u003e applied by hand or machine.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eContact and backup layer:\u003c\/strong\u003e neat as the first layer, with grog as a reinforcing layer.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eLarge moulds:\u003c\/strong\u003e from 15 cm to 2.5 metres.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eFor aluminium to bronze:\u003c\/strong\u003e suitable for the usual art casting alloys.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eDimensionally stable:\u003c\/strong\u003e linear expansion at most 0.3% after 2 hours.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Art casting of bronze and aluminium with the lost-wax method\u003c\/li\u003e\u003cli\u003e✓ First contact layer on wax models\u003c\/li\u003e\u003cli\u003e✓ Reinforcing layer with grog or aluminosilicates\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing\u003c\/h3\u003e\u003col\u003e\u003cli\u003eWeigh powder and water accurately: 42% water based on the powder weight. Work with clean materials and preferably mix under vacuum.\u003c\/li\u003e\u003cli\u003eMix for approx. 4 minutes, long enough for a homogeneous mixture.\u003c\/li\u003e\u003cli\u003eApply the investment by hand or machine within the working time of approx. 13 minutes. Make sure the mixture does not become too thick or too stiff. After approx. 17 minutes the investment starts to set.\u003c\/li\u003e\u003cli\u003eUse the neat investment as the first layer, then build up a reinforcing layer of HYDRACAST Tradition with grog or another filler.\u003c\/li\u003e\u003cli\u003eLet the mould set undisturbed and wait at least 2 hours before dewaxing or firing.\u003c\/li\u003e\u003cli\u003eDewaxing: under moist conditions at 100 °C or dry at 150 to 160 °C, for 6 to 8 hours. Above 400 °C the wax residues also burn off, which reduces casting defects.\u003c\/li\u003e\u003cli\u003eFiring cycle: raise to 200 °C as quickly as possible and allow 2 to 8 hours there for dewaxing, depending on size. Then raise by 100 to 120 °C per hour to 700 to 750 °C and hold that temperature for approx. 1 hour per 1 to 2 cm of mould radius. Cool very slowly, at no more than 70 °C per hour.\u003c\/li\u003e\u003c\/ol\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ The powder can release dust containing crystalline silica. Work with as little dust as possible, with extraction or good ventilation, and wear a dust mask (FFP2 or FFP3).\u003c\/li\u003e\u003cli\u003e✓ All water must be removed from the mould before you pour metal. The drying time depends strongly on the thickness and the number of moulds in the kiln.\u003c\/li\u003e\u003cli\u003e✓ The powder-to-water ratio affects setting time and strength, so always weigh accurately.\u003c\/li\u003e\u003cli\u003e✓ Plaster products are not suitable for outdoor use or very damp locations.\u003c\/li\u003e\u003cli\u003e✓ Store in the original 25 kg bag, dry and frost-free. The shelf life is then 12 months.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure which investment or firing cycle suits your model? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"GRS Goodwin","offers":[{"title":"Hydracast Tradition [25 kg]","offer_id":49531888664917,"sku":"A10112","price":65.55,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/grs-goodwin-hydracast-tradition-48098058109269.jpg?v=1727353848"},{"product_id":"creart","title":"GRS HYDRACAST Cre'Art – Fine-Grained Investment for Art Casting in Bronze \u0026 Copper Alloys","description":"\u003ch2\u003eFine-grained investment for art casting in bronze and copper alloys\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eGRS HYDRACAST Cre'Art\u003c\/strong\u003e is a ready-to-use, fine-grained, plaster-based refractory investment, specially formulated for art foundries. It is used to make ornamental castings of 20 cm to 1 metre in copper alloys such as bronze, using the lost wax process. Cre'Art combines good mechanical strength with a fine surface finish and good value for money. You mix 100 parts powder with 36 parts water and have 17 minutes working time.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eFor art foundries:\u003c\/strong\u003e developed for ornamental castings in copper alloys.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eLarge pieces:\u003c\/strong\u003e from 20 cm to 1 metre.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eFine-grained:\u003c\/strong\u003e a smooth, detailed surface.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eGood strength:\u003c\/strong\u003e a sturdy mould during burnout and pouring.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eGenerous working time:\u003c\/strong\u003e 17 minutes to mix and pour.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Art casting of bronze and other copper alloys with the lost wax process\u003c\/li\u003e\u003cli\u003e✓ Ornamental castings of 20 cm to 1 metre\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing (per the GRS TDS)\u003c\/h3\u003e\u003col\u003e\u003cli\u003eWeigh powder and water precisely: 100 parts powder to 36 parts water. The ratio can be adjusted by 1 part to suit your application.\u003c\/li\u003e\u003cli\u003eUse clean equipment and preferably mix under vacuum, for about 4 minutes.\u003c\/li\u003e\u003cli\u003ePour immediately after mixing, within the 17 minute working time. Let the mix flow slowly over the model so no air is trapped. Vacuum casting prevents air bubbles.\u003c\/li\u003e\u003cli\u003eDo not handle the mould before it has set (24 to 28 minutes) and wait at least 2 hours before starting the heat treatment.\u003c\/li\u003e\u003cli\u003eDewaxing: with steam at about 100 °C or dry at 150 to 160 °C, for 6 to 8 hours. Above 400 °C the last traces of wax are removed, giving a perfect interior surface.\u003c\/li\u003e\u003cli\u003eStandard art foundry firing cycle: heat at 100 °C per hour to 250 °C and hold for 6 to 8 hours. Heat at 150 °C per hour to 760 °C and hold for 6 to 8 hours. Cool at 100 °C per hour to the desired casting temperature.\u003c\/li\u003e\u003cli\u003eAfter casting, let the mould cool and break it away by immersion in water or with a high-pressure cleaner.\u003c\/li\u003e\u003c\/ol\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Cre'Art is developed for metal. For glass and pâte de verre, use \u003ca href=\"\/en\/products\/crystalcast\"\u003eCrystalcast M248\u003c\/a\u003e.\u003c\/li\u003e\u003cli\u003e✓ All water must be removed from the mould before pouring metal. Drying time depends heavily on the size and number of moulds in the kiln.\u003c\/li\u003e\u003cli\u003e✓ The powder may release dust containing crystalline silica. Work dust-free, with extraction or good ventilation, and wear a dust mask.\u003c\/li\u003e\u003cli\u003e✓ Store dry and frost-free in the original bag and use the oldest stock first. Shelf life 12 months when stored dry.\u003c\/li\u003e\u003cli\u003e✓ Supplied in 25 kg bags.\u003c\/li\u003e\u003c\/ul\u003e\u003cp\u003eSee all \u003ca href=\"\/en\/collections\/plaster-investment-lost-wax-casting\"\u003einvestments for lost wax casting\u003c\/a\u003e.\u003c\/p\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure which investment or firing cycle suits your model? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"GRS Goodwin","offers":[{"title":"HYDRACAST ™ Cre'Art - 25 kg","offer_id":49531889287509,"sku":"A10109","price":98.95,"currency_code":"EUR","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/grs-goodwin-hydracast-creart-48098057978197.jpg?v=1727353848"},{"product_id":"zirkoon-zand-en-meel-gecalcineerd","title":"Calcined Zircon Flour and Sand","description":"\u003cp\u003e\u003cstrong\u003eDiscover the Strength of Zircon Sand and Flour for the Ceramic Shell Process!\u003c\/strong\u003e\u003c\/p\u003e\n\u003cp\u003eLooking for high-quality materials for your ceramic projects? Look no further! Our zircon sand and flour are the ideal solution for the ceramic shell process, renowned for its exceptional durability and aesthetic quality.\u003c\/p\u003e\n\u003cp\u003e\u003cstrong\u003eWhy choose our zircon sand and flour?\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cp\u003e\u003cstrong\u003eSuperior Quality\u003c\/strong\u003e: Our zircon sand and flour are carefully selected and processed to ensure the highest purity and consistency.\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli\u003e\n\u003cp\u003e\u003cstrong\u003eExcellent Thermal Stability\u003c\/strong\u003e: Ideal for high-temperature applications, so your ceramic creations withstand extreme conditions.\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli\u003e\n\u003cp\u003e\u003cstrong\u003eIncreased Strength and Durability\u003c\/strong\u003e: Reinforce your ceramic products with the robust properties of zircon for a longer service life and better performance.\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli\u003e\n\u003cp\u003e\u003cstrong\u003eVersatile Use\u003c\/strong\u003e: Ideal for a wide range of ceramic applications, from artworks to industrial components.\u003c\/p\u003e\n\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eApplications:\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cp\u003e\u003cstrong\u003eCeramic Shells\u003c\/strong\u003e: Create fine, durable ceramic shells that stand the test of time.\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli\u003e\n\u003cp\u003e\u003cstrong\u003eIndustrial Use\u003c\/strong\u003e: Ideal for making refractory materials and for other industrial applications.\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli\u003e\n\u003cp\u003e\u003cstrong\u003eArtistic Projects\u003c\/strong\u003e: Give your artworks a distinctive look and improved durability.\u003c\/p\u003e\n\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cbr\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cstrong\u003eZircon Sand 108-13 Mesh\u003c\/strong\u003e\u003c\/p\u003e\n\u003cp\u003eTypical chemical analysis\u003cbr\u003eZrO2 66.2%\u003cbr\u003eSiO2 32%\u003cbr\u003eFe2O3 \u0026lt; 0.06%\u003cbr\u003eAl2O3 \u0026lt; 0.5%\u003cbr\u003eTiO2 \u0026lt; 0.15%\u003cbr\u003eCaO \u0026lt; 0.05%\u003cbr\u003eMgO \u0026lt; 0.1%\u003cbr\u003eNa2O \u0026lt; 0.02%\u003cbr\u003eK2O \u0026lt; 0.02%\u003c\/p\u003e\n\u003cp\u003ePhysical properties\u003c\/p\u003e\n\u003cp\u003eSpecific gravity [kg\/dm³] 4.6\u003cbr\u003eHardness [Mohs] 7.5\u003cbr\u003eMelting point [°C] 2200\u003c\/p\u003e\n\u003cp\u003e\u003cbr\u003eGrain size distribution\u003c\/p\u003e\n\u003cp\u003e\u0026gt; 0.315 mm ---\u003cbr\u003e\u0026gt; 0.250 mm 0.04%\u003cbr\u003e\u0026gt; 0.200 mm 0.38%\u003cbr\u003e\u0026gt; 0.150 mm 7.02%\u003cbr\u003e\u0026gt; 0.125 mm 18.19%\u003cbr\u003e\u0026gt; 0.100 mm 54.52%\u003cbr\u003e\u0026gt; 0.090 mm 11.52%\u003cbr\u003e\u0026lt; 0.090 mm 8.58%\u003c\/p\u003e\n\u003cp\u003e\u003cbr\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cstrong\u003eZircon Flour 200 Mesh\u003c\/strong\u003e\u003c\/p\u003e\n\u003cp\u003eTypical chemical and physical properties:\u003cbr\u003eChemical analysis: typical \/ guaranteed\u003cbr\u003eProperties\u003cbr\u003eZirconia (incl. hafnia) ZrO2 (+HfO2): typical 66.40%, guaranteed 64.00% min.\u003cbr\u003eSilica SiO2: typical 32.60%, guaranteed 34.00% max.\u003cbr\u003eTitania TiO2: typical 0.17%, guaranteed 0.23% max.\u003cbr\u003eAlumina Al2O3: typical 0.62%, guaranteed 1.00% max.\u003cbr\u003eIron oxide Fe2O3: typical 0.06%, guaranteed 0.10% max.\u003cbr\u003e\u003cbr\u003e\u003c\/p\u003e\n\u003cp\u003eTypical physical properties:\u003cbr\u003eSpecific gravity 4.65 g\/cm³\u003cbr\u003eHardness (Mohs) 7.5\u003cbr\u003eMelting temperature 2,200 °C\u003cbr\u003eMoisture 0.09%\u003cbr\u003eLoss on ignition 0.35%\u003c\/p\u003e","brand":"Nedform","offers":[{"title":"Zircon Sand 108-113 mesh calcined [25 kg]","offer_id":49917163241813,"sku":"A11856","price":138.19,"currency_code":"EUR","in_stock":false},{"title":"Zirconium flour 200 mesh calcined [25 kg]","offer_id":49917163274581,"sku":"A10218","price":118.9,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/nedform-zirkoon-meel-en-zand-gecalcineerd-48720179265877.jpg?v=1732155988"},{"product_id":"clayrac-aluminosilicaat-stukko-en-meel","title":"Imerys Clayrac Aluminosilicate – Stucco \u0026 Flour for Ceramic Shell Moulds in Art Casting \u0026 Investment Casting","description":"\u003ch2\u003eAluminosilicate stucco and flour for the ceramic shell process\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eImerys Clayrac\u003c\/strong\u003e is a calcined aluminosilicate (chamotte) made from kaolinitic clay from the Charentes basin in France. You use it as stucco and as flour to build highly refractory and creep-resistant ceramic shell moulds, for example in art casting. Clayrac has a reliable particle size distribution and mineralogy and works in both alcohol- and water-based processes. Depending on the grade, it contains up to 45 % alumina.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eHighly refractory:\u003c\/strong\u003e with high creep resistance, also for steel and titanium alloys.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eDimensionally accurate:\u003c\/strong\u003e valued for its dimensional accuracy.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eExcellent backup material:\u003c\/strong\u003e according to Imerys very well suited to the backup coats of the shell.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eConsistent quality:\u003c\/strong\u003e reliable particle size distribution and mineralogy.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eAlcohol or water:\u003c\/strong\u003e suitable for both processes.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eSeveral grain sizes:\u003c\/strong\u003e lets you build the shell more efficiently.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eEasy knock-out:\u003c\/strong\u003e the shell is easy to remove after casting.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Ceramic shell moulds for art foundries\u003c\/li\u003e\u003cli\u003e✓ Investment casting, including steel and titanium alloys\u003c\/li\u003e\u003cli\u003e✓ Stucco for building up the shell\u003c\/li\u003e\u003cli\u003e✓ Clayrac P 200 mesh as flour\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing\u003c\/h3\u003e\u003col\u003e\u003cli\u003eUse Clayrac as stucco when building the shell, or as flour (200 mesh), in an alcohol- or water-based process.\u003c\/li\u003e\u003cli\u003eChoose the right grain size for each coat. Using different grain sizes lets you build the shell more efficiently.\u003c\/li\u003e\u003cli\u003eFor slurry composition, drying times and number of coats, follow the instructions for the binder you use.\u003c\/li\u003e\u003c\/ol\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Avoid creating dust and work with good extraction.\u003c\/li\u003e\u003cli\u003e✓ Supplied in 25 kg bags. For larger quantities or delivery outside the Benelux and Germany, request a quotation.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure which grain size you need for each coat? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"Imerys","offers":[{"title":"Clayrac F 45 0.1\/0.3 mm [25 kg]","offer_id":49917163340117,"sku":"A11759","price":42.31,"currency_code":"EUR","in_stock":true},{"title":"Clayrac F 41 0.2\/0.5 mm [25 kg]","offer_id":49917163372885,"sku":"A10421","price":40.0,"currency_code":"EUR","in_stock":true},{"title":"Clayrac F 45 0,5\/1 mm [25 kg]","offer_id":49917163405653,"sku":"A10423","price":47.48,"currency_code":"EUR","in_stock":true},{"title":"Clayrac F 45 P 200 mesh [25 kg]","offer_id":49917163438421,"sku":"A11703","price":49.68,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/imerys-clayrac-aluminosilicaat-stukko-en-meel-48720179200341.png?v=1732155988"},{"product_id":"shellspen-suspensiepoeder","title":"Shellspen Suspension Powder – Stable Ceramic Slurry for Lost Wax Casting without Constant Stirring","description":"\u003ch2\u003eSuspension powder for a ceramic slurry that does not need continuous stirring\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eShellspen suspension powder\u003c\/strong\u003e was developed for ceramic slurries in the lost wax method. You dry-mix the powder through the flour and add it to the binder together with the flour. This keeps the solids in suspension much longer, so periodic mixing according to a fixed schedule is sufficient instead of a continuously rotating tank. One 250 g bag is enough for 25 kg of fused silica flour 325 mesh, i.e. a batch of 25 kg Adbond and 25 kg flour. This yields approximately 27 to 33 litres of slurry.\u003c\/p\u003e\u003ch3\u003eMain advantages\u003c\/h3\u003e\u003cul\u003e\n\u003cli\u003e\u003cstrong\u003eNo continuously rotating tank:\u003c\/strong\u003e periodic mixing according to schedule is sufficient.\u003c\/li\u003e\n\u003cli\u003e\u003cstrong\u003eStable slurry:\u003c\/strong\u003e the solids stay in suspension longer, so the slurry remains homogeneous.\u003c\/li\u003e\n\u003cli\u003e\u003cstrong\u003eFull control:\u003c\/strong\u003e you prepare the slurry yourself from binder, flour and Shellspen.\u003c\/li\u003e\n\u003cli\u003e\u003cstrong\u003eBronze and aluminium:\u003c\/strong\u003e the slurry can be used for both metals.\u003c\/li\u003e\n\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\n\u003cli\u003e✓ Ceramic shell for the lost wax method\u003c\/li\u003e\n\u003cli\u003e✓ Professional users without a continuously rotating slurry tank\u003c\/li\u003e\n\u003cli\u003e✓ Bronze and aluminium casting\u003c\/li\u003e\n\u003c\/ul\u003e\u003ch3\u003eProcessing\u003c\/h3\u003e\u003col\u003e\n\u003cli\u003eTake 25 kg of fused silica flour 325 mesh.\u003c\/li\u003e\n\u003cli\u003eDry-mix the entire contents of one bag of Shellspen through the flour.\u003c\/li\u003e\n\u003cli\u003ePour 25 kg of Adbond (approx. 21 litres) into a clean container of at least 40 litres.\u003c\/li\u003e\n\u003cli\u003eAdd the dry mixture of flour and Shellspen to the Adbond through a sieve while mixing.\u003c\/li\u003e\n\u003cli\u003eMix with a powerful mixer at low speed (maximum 2000 revolutions per minute) until no dry grains remain on the bottom, then continue mixing intensively: at least 4 hours, preferably 24 hours.\u003c\/li\u003e\n\u003cli\u003eLet the slurry rest overnight, mix again and sieve the slurry.\u003c\/li\u003e\n\u003cli\u003eCheck density, viscosity and pH (always above 9.5) and record the values in a logbook.\u003c\/li\u003e\n\u003cli\u003eThe complete procedure is described in the \u003ca href=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/Manual_periodically_mixed_slurry_shellspen_EN_d8ed81e9-56b4-44d9-a0ea-a03ea3f9a7b9.pdf?v=1792407027\" target=\"_blank\" rel=\"noopener\"\u003emanual for periodically mixed slurry based on Shellspen (PDF)\u003c\/a\u003e. Read it in full before you start.\u003c\/li\u003e\n\u003c\/ol\u003e\u003ch3\u003eMixing schedule\u003c\/h3\u003e\u003cul\u003e\n\u003cli\u003e✓ On every day of use: mix for about half an hour before measuring, and always thoroughly just before dipping.\u003c\/li\u003e\n\u003cli\u003e✓ During periods without use (weekend, holidays): mix for half an hour at least twice a week. Never leave the slurry unmixed for more than 7 days.\u003c\/li\u003e\n\u003cli\u003e✓ How long a prepared slurry remains usable depends entirely on maintenance (mixing schedule, pH, temperature, hygiene). No guarantee is given on the life of a prepared slurry.\u003c\/li\u003e\n\u003c\/ul\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\n\u003cli\u003e✓ This is a separate formulation with finer flour (325 mesh instead of the usual 120 or 200 mesh), not the same slurry stirred less often.\u003c\/li\u003e\n\u003cli\u003e✓ Start on the thin side (1:1). Thicken with flour plus the corresponding Shellspen, thin with Adbond. Do not add water to rescue a thick slurry; only top up evaporated water with demineralised water.\u003c\/li\u003e\n\u003cli\u003e✓ Storage: Adbond binder at 5–30 °C, the prepared slurry at 15–25 °C (never below 5 °C or above 30 °C), frost-free and sealed.\u003c\/li\u003e\n\u003cli\u003e✓ If you only use part of a bag, homogenise the powder thoroughly first and add a proportional amount.\u003c\/li\u003e\n\u003cli\u003e✓ Always rinse degreased models with demineralised water.\u003c\/li\u003e\n\u003cli\u003e✓ For aluminium we recommend Clayrac (aluminium silicate) as stucco, as a full fused silica shell can be harder to remove.\u003c\/li\u003e\n\u003cli\u003e✓ This product is intended for professional users. An overview of all options can be found on the collection page \u003ca href=\"\/en\/collections\/ceramic-shell-materials-for-the-lost-wax-method\"\u003eCeramic shell materials\u003c\/a\u003e.\u003c\/li\u003e\n\u003c\/ul\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure which ceramic shell build-up suits your casting work? Email us at info@siliconesandmore.com and we will be happy to advise you.\u003c\/p\u003e","brand":"Shellspen","offers":[{"title":"250 gram bag for 25 kg flour or 50 kg slurry","offer_id":49923622306133,"sku":"A11995","price":110.11,"currency_code":"EUR","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/shellspen-shellspen-suspensiepoeder-48730437058901.jpg?v=1732266034"},{"product_id":"droogindicator-voor-keramische-schaal","title":"Drying Indicator for Ceramic Shell","description":"\u003cp\u003eAcid Yellow is a dye used as a drying indicator in the ceramic shell method. The dye changes colour as the slurry dries, so you can visually judge when a layer is dry enough to apply the next one.\u003c\/p\u003e\n\u003cp\u003e\u003cstrong\u003eUse\u003c\/strong\u003e\u003c\/p\u003e\n\u003cp\u003eDose \u003cstrong\u003ea maximum of 100 ml drying indicator per 25 kg Adbond binder\u003c\/strong\u003e (4 ml per kg Adbond). Do not use more, even if you have a larger pack.\u003c\/p\u003e\n\u003cp\u003e\u003cstrong\u003ePLEASE NOTE\u003c\/strong\u003e\u003c\/p\u003e\n\u003cp\u003eThis dye is a salt and makes the slurry less stable. Its use is optional and not recommended for beginners. Do not use drying indicator in a slurry that already shows problems (thickening, deviating pH). A dry layer can also be recognised by a lighter, more matt colour, or measured with a moisture meter.\u003c\/p\u003e\n\u003cp\u003eSee the manuals on the collection page \u003ca href=\"\/en\/collections\/ceramic-shell-materials-for-the-lost-wax-method\"\u003eCeramic shell materials\u003c\/a\u003e for the complete process.\u003c\/p\u003e","brand":"Nedform","offers":[{"title":"1 bottle yellow dryness indicator liquid [1 Liter]","offer_id":49923622338901,"sku":"S11604","price":42.35,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/nedform-droogindicator-keramische-schaal-48730436927829.jpg?v=1732266034"},{"product_id":"hydracast-™-m463p","title":"GRS HYDRACAST M463P – Investment \u0026 Core Material for Lost Wax and Vacuum Casting of Aluminium","description":"\u003ch2\u003eInvestment and core material for lost wax casting\u003c\/h2\u003e\u003cp\u003e\u003cstrong\u003eGRS HYDRACAST M463P\u003c\/strong\u003e is a plaster-based investment for the lost wax process. You pour it into a flask around the wax patterns. M463P was developed specifically for large, thin-walled castings in aluminium and other low-temperature non-ferrous alloys cast under vacuum. Its high green strength and good thermal shock resistance make it especially suitable for larger castings with troublesome cores. Mixing ratio 100 parts powder to 28 parts water, working time 23 minutes.\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003eAlso as a core material.\u003c\/strong\u003e You can also use M463P to cast cores for hollow castings. Its high green strength keeps the core strong enough to handle and position in the mould.\u003c\/p\u003e\u003ch3\u003eKey benefits\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eInvestment and core material:\u003c\/strong\u003e one plaster for the mould and the cores.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eHigh green strength:\u003c\/strong\u003e once set, the mould is strong enough for large patterns and troublesome cores.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eGood thermal shock resistance:\u003c\/strong\u003e reliable during dewaxing and burnout.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eFor vacuum casting:\u003c\/strong\u003e developed for aluminium and other low-temperature non-ferrous alloys under vacuum.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eGenerous working time:\u003c\/strong\u003e 23 minutes to mix, vacuum and pour.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eTypical applications\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ Core material for making cores in hollow castings\u003c\/li\u003e\u003cli\u003e✓ Lost wax casting of aluminium under vacuum\u003c\/li\u003e\u003cli\u003e✓ Other low-temperature non-ferrous alloys\u003c\/li\u003e\u003cli\u003e✓ Large, thin-walled castings with troublesome cores\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003eProcessing (per the GRS TDS)\u003c\/h3\u003e\u003cp\u003e\u003cstrong\u003eConventional mixing\u003c\/strong\u003e\u003c\/p\u003e\u003col\u003e\u003cli\u003eAdjust the water temperature to give a slurry temperature of 20 °C.\u003c\/li\u003e\u003cli\u003eAdd the powder to the water (100 : 28 by weight) and hand-mix for 30 seconds.\u003c\/li\u003e\u003cli\u003eThen machine-mix for 4 minutes.\u003c\/li\u003e\u003cli\u003eVacuum the bowl for no more than 3 minutes.\u003c\/li\u003e\u003cli\u003ePour slowly down the side of the flask until the patterns are covered.\u003c\/li\u003e\u003cli\u003eVacuum the flask for no more than 3 minutes.\u003c\/li\u003e\u003c\/ol\u003e\u003cp\u003e\u003cstrong\u003eVacuum mixing\u003c\/strong\u003e\u003c\/p\u003e\u003col\u003e\u003cli\u003eAdjust the water temperature to give a slurry temperature of 20 °C.\u003c\/li\u003e\u003cli\u003eMix under vacuum for 5 minutes.\u003c\/li\u003e\u003cli\u003eFill the flasks in the investing chamber, release the vacuum and remove the flasks after 10 minutes in total.\u003c\/li\u003e\u003c\/ol\u003e\u003cp\u003eWith both methods, let the flasks stand undisturbed for at least 2 hours. Then remove the sprue base and collar.\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003eDewax and burnout\u003c\/strong\u003e\u003c\/p\u003e\u003cul\u003e\u003cli\u003e\u003cstrong\u003eWith steam (preferred):\u003c\/strong\u003e steam dewax in an autoclave at no more than 0.7 bar. Place the mould in a furnace at room temperature, heat to 200 °C at no more than 200 °C per hour and soak for 3 to 4 hours. Then heat to 700 °C at no more than 100 °C per hour.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eWithout steam:\u003c\/strong\u003e place the mould in a furnace preheated to 150 °C and soak for 5 to 7 hours. Then heat to 700 °C at no more than 100 °C per hour.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eHold at 700 °C:\u003c\/strong\u003e depends on load and flask size, typically about 5 hours for 25 × 25 × 25 cm up to 16 hours for 50 × 50 × 50 cm.\u003c\/li\u003e\u003cli\u003e\u003cstrong\u003eCooling:\u003c\/strong\u003e cool at 100 °C per hour to the mould casting temperature. For aluminium this is typically 280 to 400 °C.\u003c\/li\u003e\u003c\/ul\u003e\u003ch3\u003ePoints to note\u003c\/h3\u003e\u003cul\u003e\u003cli\u003e✓ As an investment, not suitable for metals melting above 1100 °C. For bronze, choose \u003ca href=\"\/en\/products\/hydracast-tradition\"\u003eHYDRACAST Tradition\u003c\/a\u003e, \u003ca href=\"\/en\/products\/creart\"\u003eHYDRACAST Cre'Art\u003c\/a\u003e or the \u003ca href=\"\/en\/collections\/ceramic-shell-materials-for-the-lost-wax-method\"\u003eceramic shell\u003c\/a\u003e.\u003c\/li\u003e\u003cli\u003e✓ Not recommended for casting magnesium.\u003c\/li\u003e\u003cli\u003e✓ Contains silica: do not breathe the dust and wear at least an FFP2 mask.\u003c\/li\u003e\u003cli\u003e✓ Store dry and use in rotation. Moisture and prolonged storage cause deterioration.\u003c\/li\u003e\u003cli\u003e✓ Supplied in 25 kg bags.\u003c\/li\u003e\u003c\/ul\u003e\u003cp\u003eSee all \u003ca href=\"\/en\/collections\/plaster-investment-lost-wax-casting\"\u003einvestments for lost wax casting\u003c\/a\u003e.\u003c\/p\u003e\u003ch3\u003eProfessional support\u003c\/h3\u003e\u003cp\u003eNot sure which investment or core material suits your alloy or casting method? Email us at info@siliconesandmore.com and we will be happy to help.\u003c\/p\u003e","brand":"GRS Goodwin","offers":[{"title":"HYDRACAST™ M463P [25 kg]","offer_id":51589027234133,"sku":"A90549","price":94.8,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0896\/4096\/0341\/files\/grs-goodwin-hydracast-m463p-professioneel-kerngips-voor-verloren-wa-48098057945429.jpg?v=1773846332"}],"url":"https:\/\/siliconesandmore.com\/en\/collections\/ceramic-shell-and-investment.oembed","provider":"siliconesandmore","version":"1.0","type":"link"}